Bitte benutzen Sie diese Referenz, um auf diese Ressource zu verweisen:
doi:10.22028/D291-24495 | Titel: | Photochromic coatings derived by sol-gel processing from epoxysilane, bisphenol-a, 1-methylimidazole and spirooxazine |
| VerfasserIn: | Hoffmann, Bernd Mennig, Martin Schmidt, Helmut K. Hou, Lisong |
| Sprache: | Englisch |
| Erscheinungsjahr: | 1995 |
| Quelle: | Proceedings of XVII International Congress on Glass : [Beijing, China, Oct. 9 - 14, 1995] / [organized by:] Chinese Ceramic Society. [Sponsored by: International Commission on Glass. Chief ed.: Gong Fangtian]. — Vol. 4. - Beijing : International Academic Publishers, 1995, S. 399-404 |
| Kontrollierte Schlagwörter: | Photochromie Sol-Gel-Verfahren Epoxysilane Spirooxazine |
| DDC-Sachgruppe: | 620 Ingenieurwissenschaften und Maschinenbau |
| Dokumenttyp: | Konferenzbeitrag (in einem Konferenzband / InProceedings erschienener Beitrag) |
| Abstract: | As photochromic organic dyes in solution suffer from heavy aggregation and poor thermal and phtochemical stability, solid matrices are preferred as their hosts. The low-temperature wet-chemical characteristics of the sol-gel process, fortunately, offer vast possibilities for the incorporation of organic dyes into solid matrices. In this work we present our experimental results on photochromic coatings cotaining 1,3,3-trimethyl-spiro[indoline-2,3'-[3H]naphth[2,1-b][1,4]oxazine] (SO) and derived from 3-glycidyloxypropytrimehtoxysilane (GPTMS), bisphenol-A (BPA) and 1-methylimidazole (MI) by sol-gel processing. The experimental results of the investigation of the photochromic properties as a function of matrix composition and additives include four main aspects in terms of the photochromic intensity (DeltaA0) at the photostationary state under UV irradiation and the half-life time (t0.5) of the coloured form after cessation of the UV irradiation: (1) heat treatment temperature for densification of the coatings has a great effect on DeltaAk0. (2) The BPA content shows a significant effect on both DeltaA0 and t0.5. WHile there exists an optimal content of BPA for DeltaA0, there is a steadily increase in t.05 with increasing BPA content. (3) The most encouraging result is that we are now able to increase the dye concentration in our samples to a similar concentration as is used in dye-polymer systems but with better photochromic intensity (4) The effect of additives, e.g. fluorosilnae (FAS), is also attractive to further work, because the addition of FAS not only leads to a further increase in DeltaA0 but also greatly enhances the photostability. |
| Link zu diesem Datensatz: | urn:nbn:de:bsz:291-scidok-28053 hdl:20.500.11880/24551 http://dx.doi.org/10.22028/D291-24495 |
| ISBN: | 7-8000-3343-0 |
| Datum des Eintrags: | 23-Mär-2010 |
| Fakultät: | SE - Sonstige Einrichtungen |
| Fachrichtung: | SE - INM Leibniz-Institut für Neue Materialien |
| Sammlung: | INM SciDok - Der Wissenschaftsserver der Universität des Saarlandes |
Dateien zu diesem Datensatz:
| Datei | Beschreibung | Größe | Format | |
|---|---|---|---|---|
| sm199513.pdf | 255,17 kB | Adobe PDF | Öffnen/Anzeigen |
Alle Ressourcen in diesem Repository sind urheberrechtlich geschützt.